Chip mark, diagonal grain, torn grain and wane are the defects in timber due to:
1. conversion
2. insects
3. natural forces
4. fungi

1 Answer

0 votes
by (115k points)
selected by
 
Best answer
Correct Answer - Option 1 : conversion

Defects due to conversion

1) chip mark

2) Diagonal grain

3) Torn grain

4) wane

Defects due to Insect

1) Marine Borers

2) Beetles

3) Termites

Defect due to Fungi

1) Blue Rot

2) Heart Rot

3) Dry Rot

4) Sap stain

5) Wet Rot

Defect due to seasoning

1) Bow

2) check

3) collapse

4) cup

5) Twist

6) Split

7) Warp

Defects due to natural forces

1) knots

2) Burb

3) Ring galls

4) Twisted fiber

5) shaker

6) Druxinees

Welcome to Sarthaks eConnect: A unique platform where students can interact with teachers/experts/students to get solutions to their queries. Students (upto class 10+2) preparing for All Government Exams, CBSE Board Exam, ICSE Board Exam, State Board Exam, JEE (Mains+Advance) and NEET can ask questions from any subject and get quick answers by subject teachers/ experts/mentors/students.