337 views
in Alkali and Alkaline Earth Metals by (45.7k points)

Which can be used in controlling galvanic corrosion? 

(a) Iron 

(b) Magnesium 

(c) Calcium 

(d) Beryllium

Please log in or register to answer this question.

1 Answer

+1 vote
by (45.0k points)

Answer: (c) Calcium

Welcome to Sarthaks eConnect: A unique platform where students can interact with teachers/experts/students to get solutions to their queries. Students (upto class 10+2) preparing for All Government Exams, CBSE Board Exam, ICSE Board Exam, State Board Exam, JEE (Mains+Advance) and NEET can ask questions from any subject and get quick answers by subject teachers/ experts/mentors/students.

...